AlMgSc Scalmalloy High-Strength Aluminum Powder
✓ VerifiedAluminum Alloy · AlMgSc (Scalmalloy) · 20-63 μm
Price Range / 价格区间
$171.00 - $213.50 / per kgMOQ: 5 kg
Lead Time: 14-21 days
● In Stock
Supplier / 供应商
L
LBPF Technology
Suzhou, China
ISO 9001
Technical Specifications / 技术规格
Chemical: Al Bal, Mg 4.0-5.0%, Sc 0.6-0.8%, Zr 0.2-0.4% | PSD: 20-63 μm | UTS: >=520 MPa | YS: >=480 MPa | Elongation: 8-13% | Density: ~2.67 g/cm³
Description / 产品描述
High-performance AlMgSc (Scalmalloy) aluminum-magnesium-scandium alloy powder. Airbus-licensed formulation with exceptional strength-to-weight ratio. Premium choice for aerospace and racing.