Ti-6Al-4V ELI Grade 23 Medical Powder

✓ Verified

Titanium Alloy · Ti-6Al-4V ELI (Grade 23) · 15-53 μm

Price Range / 价格区间

$159.00 - $191.50 / per kg

MOQ: 5 kg

Lead Time: 10-14 days

● In Stock

Request Quote →
Grade
Ti-6Al-4V ELI (Grade 23)
Particle Size
15-53 μm
Process
EIGA

Grade + Particle Size + Production Process determine pricing

Supplier / 供应商

A

Avimetal Powder Technology

Jiangsu, China

Verified
ISO 9001 AS9100D ISO 13485

Technical Specifications / 技术规格

Chemical: Ti Bal, Al 5.50-6.50%, V 3.50-4.50%, O <=0.13% (ELI) | PSD: 15-53 μm | UTS: >=860 MPa | YS: >=795 MPa | Elongation: >=10% | Biocomp: ISO 10993, ASTM F136

Description / 产品描述

Ultra-low interstitial (ELI) Ti-6Al-4V Grade 23 powder for medical implant applications. Reduced oxygen content for improved ductility and fracture toughness.