AlSi10Mg Aluminum Alloy Powder for Additive Manufacturing
✓ VerifiedAluminum Alloy · AlSi10Mg Aluminum Alloy · 15-53μm
Price Range / 价格区间
$13.50 - $16.50 / per kgMOQ: 10 kg
Lead Time: 7-14 days
● In Stock
Technical Specifications / 技术规格
Grade: AlSi10Mg Aluminum Alloy | PSD: 15-53μm | Process: NULL
Description / 产品描述
Premium AlSi10Mg Aluminum Alloy powder. ,,