316L Stainless Steel Powder for Additive Manufacturing

✓ Verified

Stainless Steel · 316L Stainless Steel · 15-53μm

Price Range / 价格区间

$8.50 - $9.00 / per kg

MOQ: 10 kg

Lead Time: 7-14 days

● In Stock

Technical Specifications / 技术规格

Grade: 316L Stainless Steel | PSD: 15-53μm | Process: NULL

Description / 产品描述

Premium 316L Stainless Steel powder. ,