TA15 Titanium Alloy Powder for Additive Manufacturing

✓ Verified

Titanium Alloy · TA15 Titanium Alloy · 75-250μm

Price Range / 价格区间

$46.00 - $49.00 / per kg

MOQ: 10 kg

Lead Time: 7-14 days

● In Stock

Request Quote →
Grade
TA15 Titanium Alloy
Particle Size
75-250μm
Process
NULL

Grade + Particle Size + Production Process determine pricing

Technical Specifications / 技术规格

Grade: TA15 Titanium Alloy | PSD: 75-250μm | Process: NULL

Description / 产品描述

Premium TA15 Titanium Alloy powder. //