High Purity Spherical Aluminum Powder
Other · 高纯 80-150目 · +60 mesh:0, -150 mesh: ≤35%
Price Range / 价格区间
$0.00 - $0.00 / per kgMOQ: 10 kg
Lead Time: 7-14 days
● In Stock
Request Quote →
Grade
高纯 80-150目
Particle Size
+60 mesh:0, -150 mesh: ≤35%
Process
N/A
Grade + Particle Size + Production Process determine pricing
Supplier / 供应商
A
Avimetal Powder Technology
Jiangsu, China
Technical Specifications / 技术规格
Grade: 80-150 | PSD: +60 mesh:0, -150 mesh: <=35%
Description / 产品描述
High Purity Spherical Aluminum Powder