1 USD = 6.80 CNY | Source: ExchangeRate-API | View Price Index →
🔬

Fine Spherical Aluminum Powder

Other · FLPN1.5 · 1.5±0.5

Price Range / 价格区间

$0.00 - $0.00 / per kg

MOQ: 10 kg

Lead Time: 7-14 days

● In Stock

Request Quote →
Grade
FLPN1.5
Particle Size
1.5±0.5
Process
N/A

Grade + Particle Size + Production Process determine pricing

Supplier / 供应商

A

Avimetal Powder Technology

Jiangsu, China

Verified

Technical Specifications / 技术规格

Grade: FLPN1.5 | PSD: 1.5+/-0.5

Description / 产品描述

Fine Spherical Aluminum Powder