Fine Spherical Aluminum Powder

Other · 80-150目 · +60 mesh: 0, -150 mesh: ≤35%

Price Range / 价格区间

$0.00 - $0.00 / per kg

MOQ: 10 kg

Lead Time: 7-14 days

● In Stock

Request Quote →
Grade
80-150目
Particle Size
+60 mesh: 0, -150 mesh: ≤35%
Process
N/A

Grade + Particle Size + Production Process determine pricing

Supplier / 供应商

A

Avimetal Powder Technology

Jiangsu, China

Verified

Technical Specifications / 技术规格

Grade: 80-150 | PSD: +60 mesh: 0, -150 mesh: <=35%