Ag-Cu-Zn-Sn Powder
Other · 4N银铜锌锡合金粉 · -300目,-500目
Price Range / 价格区间
$0.00 - $0.00 / per kgMOQ: 10 kg
Lead Time: 7-14 days
● In Stock
Request Quote →
Grade
4N银铜锌锡合金粉
Particle Size
-300目,-500目
Process
气雾化(VIGA)
Grade + Particle Size + Production Process determine pricing
Supplier / 供应商
A
Avimetal Powder Technology
Jiangsu, China
Technical Specifications / 技术规格
Grade: 4N | PSD: -300,-500 | Process: (VIGA)
Description / 产品描述
Ag-Cu-Zn-Sn Powder