SUPERFLOW® Ti-6AI-4V

Titanium Alloy · Ti-6Al-4V (Grade 5) · 15-53μm

Price Range / 价格区间

$0.00 - $0.00 / per kg

MOQ: 10 kg

Lead Time: 7-14 days

● In Stock

Supplier / 供应商

A

Avimetal Powder Technology

Jiangsu, China

Verified

Technical Specifications / 技术规格

Grade: Ti-6Al-4V (Grade 5) | PSD: 15-53μm | Process: (

Description / 产品描述

SUPERFLOW® Ti-6AI-4V Suitable for