SUPERFLOW® Ti-6AI-4V
Titanium Alloy · Ti-6Al-4V (Grade 5) · 20-63μm
Price Range / 价格区间
$0.00 - $0.00 / per kgMOQ: 10 kg
Lead Time: 7-14 days
● In Stock
Supplier / 供应商
A
Avimetal Powder Technology
Jiangsu, China
Technical Specifications / 技术规格
Grade: Ti-6Al-4V (Grade 5) | PSD: 20-63μm | Process: (
Description / 产品描述