SUPERFLOW® Ti-6.5Al-1Mo-1V-2Zr
Titanium Alloy · TA15 Titanium Alloy · 15-53μm
Price Range / 价格区间
$0.00 - $0.00 / per kgMOQ: 10 kg
Lead Time: 7-14 days
● In Stock
Request Quote →
Grade
TA15 Titanium Alloy
Particle Size
15-53μm
Process
增材制造技术(SLM/EBM)
Grade + Particle Size + Production Process determine pricing
Supplier / 供应商
A
Avimetal Powder Technology
Jiangsu, China
Technical Specifications / 技术规格
Grade: TA15 Titanium Alloy | PSD: 15-53μm | Process: (
Description / 产品描述
SUPERFLOW® Ti-6.5Al-1Mo-1V-2Zr Suitable for SLMEBM