Ti Grade1 Titanium Alloy Powder
Titanium Alloy · Ti Grade1 (ASTM B265: Gr.1; GB/T 2965: TA1) · 15-53μm
Price Range / 价格区间
$0.00 - $0.00 / per kgMOQ: 10 kg
Lead Time: 7-14 days
● In Stock
Supplier / 供应商
A
Avimetal Powder Technology
Jiangsu, China
Technical Specifications / 技术规格
Grade: Ti Grade1 (ASTM B265: Gr.1; GB/T 2965: TA1) | PSD: 15-53μm
Description / 产品描述
Ti Grade1 Titanium Alloy Powder