7075 Aluminum Alloy Powder for Additive Manufacturing
✓ VerifiedAluminum Alloy · 7075 Aluminum Alloy · 15-53um
Price Range / 价格区间
$26.50 - $38.50 / per kgMOQ: 10 kg
Lead Time: 7-14 days
● In Stock
Request Quote →
Grade
7075 Aluminum Alloy
Particle Size
15-53um
Process
NULL
Grade + Particle Size + Production Process determine pricing
Technical Specifications / 技术规格
Grade: 7075 Aluminum Alloy | PSD: 15-53um | Process: NULL
Description / 产品描述
Premium 7075 Aluminum Alloy powder. ,,