Ti-6.5Al-2Sn-1Zr -2Mo-1W-0.2Si (TC25) Titanium Alloy Powder
Aluminum Alloy · Ti-6.5Al-2Sn-1Zr -2Mo-1W-0.2Si (TC25) · 15~53μm
Price Range / 价格区间
$0.00 - $0.00 / per kgMOQ: 10 kg
Lead Time: 7-14 days
● In Stock
Supplier / 供应商
A
Avimetal Powder Technology
Jiangsu, China
Technical Specifications / 技术规格
Grade: Ti-6.5Al-2Sn-1Zr -2Mo-1W-0.2Si (TC25) | PSD: 15~53μm | Process: | Application:
Description / 产品描述
Ti-6.5Al-2Sn-1Zr -2Mo-1W-0.2Si (TC25) Titanium Alloy Powder Suitable for .