Atomized Spherical Al-Mg Alloy Powder
Aluminum Alloy · Mg-Al Alloy Powder · 80-325目 (45μm-180μm)
Price Range / 价格区间
$0.00 - $0.00 / per kgMOQ: 10 kg
Lead Time: 7-14 days
● In Stock
Request Quote →
Grade
Mg-Al Alloy Powder
Particle Size
80-325目 (45μm-180μm)
Process
雾化法
Grade + Particle Size + Production Process determine pricing
Supplier / 供应商
A
Avimetal Powder Technology
Jiangsu, China
Technical Specifications / 技术规格
Grade: Mg-Al Alloy Powder | PSD: 80-325 (45μm-180μm) | Proc
Description / 产品描述
Atomized Spherical Al-Mg Alloy Powder Suitable for