18Ni300 High-strength Steel Powder
Other · 18Ni300 Maraging Steel · 15-53μm
Price Range / 价格区间
$0.00 - $0.00 / per kgMOQ: 10 kg
Lead Time: 7-14 days
● In Stock
Request Quote →
Grade
18Ni300 Maraging Steel
Particle Size
15-53μm
Process
N/A
Grade + Particle Size + Production Process determine pricing
Supplier / 供应商
A
Avimetal Powder Technology
Jiangsu, China
Technical Specifications / 技术规格
Grade: 18Ni300 Maraging Steel | PSD: 15-53μm | Application: ,3D
Description / 产品描述
18Ni300 High-strength Steel Powder Suitable for