30CrMnSiNi2A High-strength Steel Powder
Other · 30CrMnSiNi2A · 53-150μm
Price Range / 价格区间
$0.00 - $0.00 / per kgMOQ: 10 kg
Lead Time: 7-14 days
● In Stock
Supplier / 供应商
A
Avimetal Powder Technology
Jiangsu, China
Technical Specifications / 技术规格
Grade: 30CrMnSiNi2A | PSD: 53-150μm | Application:
Description / 产品描述
30CrMnSiNi2A High-strength Steel Powder Suitable for