GH3536 High Temperature Alloy Powder
Nickel Alloy · GH3536 · 15-53μm
Price Range / 价格区间
$0.00 - $0.00 / per kgMOQ: 10 kg
Lead Time: 7-14 days
● In Stock
Technical Specifications / 技术规格
Grade: GH3536 | PSD: 15-53μm | Process: | Application:
Description / 产品描述
GH3536 High Temperature Alloy Powder Suitable for