DT4C Pure Iron Powder for Additive Manufacturing
✓ VerifiedStainless Steel · DT4C Pure Iron · 15-53μm,53-150μm
Price Range / 价格区间
$26.50 - $32.50 / per kgMOQ: 10 kg
Lead Time: 7-14 days
● In Stock
Technical Specifications / 技术规格
Grade: DT4C Pure Iron | PSD: 15-53μm,53-150μm | Process: PREP (Plasma Rotating Electrode Process)
Description / 产品描述
Premium DT4C Pure Iron powder. ,,,