H13 Hot Work Tool Steel Powder for Additive Manufacturing

✓ Verified

Stainless Steel · H13 Hot Work Tool Steel · 53-150μm

Price Range / 价格区间

$21.00 - $24.00 / per kg

MOQ: 10 kg

Lead Time: 7-14 days

● In Stock

Technical Specifications / 技术规格

Grade: H13 Hot Work Tool Steel | PSD: 53-150μm | Process: PREP (Plasma Rotating Electrode Process)

Description / 产品描述

Premium H13 Hot Work Tool Steel powder. ,,,