CuCrZr Copper Alloy Powder for Additive Manufacturing

✓ Verified

Copper Alloy · CuCrZr Copper Alloy · 15-53μm

Price Range / 价格区间

$66.50 - $71.00 / per kg

MOQ: 10 kg

Lead Time: 7-14 days

● In Stock

Technical Specifications / 技术规格

Grade: CuCrZr Copper Alloy | PSD: 15-53μm | Process: PREP (Plasma Rotating Electrode Process)

Description / 产品描述

Premium CuCrZr Copper Alloy powder. ,,,