GH4169 / Inconel 718 Nickel Superalloy Powder for Additive Manufacturing
✓ VerifiedNickel Alloy · GH4169 / Inconel 718 Nickel Superalloy · 15-53μm
Price Range / 价格区间
$44.50 - $49.00 / per kgMOQ: 10 kg
Lead Time: 7-14 days
● In Stock
Request Quote →
Grade
GH4169 / Inconel 718 Nickel Superalloy
Particle Size
15-53μm
Process
PREP (Plasma Rotating Electrode Process)
Grade + Particle Size + Production Process determine pricing
Technical Specifications / 技术规格
Grade: GH4169 / Inconel 718 Nickel Superalloy | PSD: 15-53μm | Process: PREP (Plasma Rotating Electrode Process)
Description / 产品描述
Premium GH4169 / Inconel 718 Nickel Superalloy powder. ,