AlCoCrFeNi2.1 High Entropy Alloy Powder
Aluminum Alloy · AlCoCrFeNi2.1 · 50-150μm
Price Range / 价格区间
$0.00 - $0.00 / per kgMOQ: 10 kg
Lead Time: 7-14 days
● In Stock
Supplier / 供应商
A
Avimetal Powder Technology
Jiangsu, China
Technical Specifications / 技术规格
Grade: AlCoCrFeNi2.1 | PSD: 50-150μm | Application:
Description / 产品描述
AlCoCrFeNi2.1 High Entropy Alloy Powder Suitable for