Stainless Steel 316L Powder for Industrial AM
✓ VerifiedStainless Steel · 316L · 15-53 μm
Price Range / 价格区间
$29.50 - $37.50 / per kgMOQ: 25 kg
Lead Time: 3-5 days
● In Stock
Request Quote →
Grade
316L
Particle Size
15-53 μm
Process
VIGA
Grade + Particle Size + Production Process determine pricing
Supplier / 供应商
W
Weilaray Advanced Powder
Hunan, China
ISO 9001
Technical Specifications / 技术规格
Chemical: Fe Bal, Cr 16.0-18.0%, Ni 10.0-14.0%, Mo 2.0-3.0%, C <=0.03% | PSD: 15-53 μm | App Density: >=3.9 g/cm³ | Flow: <=22 s/50g | O2: <=200 ppm | UTS: 500-670 MPa
Description / 产品描述
High-quality 316L austenitic stainless steel powder. Most widely used material in metal AM. Excellent corrosion resistance, good mechanical properties, competitive pricing.