TC11 Titanium Alloy Powder for Additive Manufacturing

✓ Verified

Titanium Alloy · TC11 Titanium Alloy · 75-250μm

Price Range / 价格区间

$50.50 - $54.50 / per kg

MOQ: 10 kg

Lead Time: 7-14 days

● In Stock

Technical Specifications / 技术规格

Grade: TC11 Titanium Alloy | PSD: 75-250μm | Process: PREP (Plasma Rotating Electrode Process)

Description / 产品描述

Premium TC11 Titanium Alloy powder. ,,,