Pure Vanadium V Spherical Powder

Other · 纯钒V · 50-150μm

Price Range / 价格区间

$0.00 - $0.00 / per kg

MOQ: 10 kg

Lead Time: 7-14 days

● In Stock

Request Quote →
Grade
纯钒V
Particle Size
50-150μm
Process
N/A

Grade + Particle Size + Production Process determine pricing

Supplier / 供应商

A

Avimetal Powder Technology

Jiangsu, China

Verified

Technical Specifications / 技术规格

Grade: V | PSD: 50-150μm | Application:

Description / 产品描述

Pure Vanadium V Spherical Powder Suitable for .