AlSi10Mg Aluminum Alloy Powder for Automotive
✓ VerifiedAluminum Alloy · AlSi10Mg · 20-63 μm
Price Range / 价格区间
$40.50 - $51.50 / per kgMOQ: 25 kg
Lead Time: 5-7 days
● In Stock
Supplier / 供应商
C
CNPC Powder Materials
Anhui, China
ISO 9001
Technical Specifications / 技术规格
Chemical: Al Bal, Si 9.0-11.0%, Mg 0.20-0.45%, Fe <=0.55% | PSD: 20-63 μm | Density: ~2.68 g/cm³ | UTS (as-built): 350-450 MPa | YS: 200-250 MPa | Elongation: 3-6%
Description / 产品描述
Cost-effective AlSi10Mg casting alloy powder for automotive lightweight components. Excellent printability, good thermal conductivity, and low density. Suitable for high-volume production.