Ti-6Al-4V Spherical Powder for Aerospace AM
✓ VerifiedTitanium Alloy · Ti-6Al-4V (Grade 5) · 15-53 μm
Price Range / 价格区间
$90.00 - $101.50 / per kgMOQ: 10 kg
Lead Time: 7-10 days
● In Stock
Supplier / 供应商
A
Avimetal Powder Technology
Jiangsu, China
ISO 9001
AS9100D
Technical Specifications / 技术规格
Chemical: Ti Bal, Al 5.50-6.75%, V 3.50-4.50%, Fe <=0.30%, O <=0.13%, N <=0.05% | PSD: D10 >=10μm, D50 30-35μm, D90 <=55μm | App Density: >=2.7 g/cm³ | Flow: <=35 s/50g | Sphericity: >=0.92 | UTS: 900-1100 MPa
Description / 产品描述
Premium grade Ti-6Al-4V (Grade 5) spherical powder optimized for SLM and EBM. Produced via EIGA process ensuring ultra-low oxygen content and excellent flowability. Ideal for aerospace structural components, medical implants, and high-performance automotive parts.