All prices are EXW (Ex-Works) factory gate prices in Chinese Yuan (CNY). USD prices are converted at the daily exchange rate for reference only. Export handling, customs documentation, special packaging, shipping, and insurance are NOT included. Contact suppliers directly for landed pricing to your destination.

Material Grade Price USD/kg (ref.) Price CNY/kg (EXW) Source
Stainless Steel 316L Stainless Steel $8.50 - $9.00 ¥58 - ¥61 Supplier quotation
EXW
Aluminum Alloy AlSi(5-70) Aluminum-Silicon Alloy $10.00 - $22.50 ¥68 - ¥153 Supplier quotation
EXW
Aluminum Alloy AlSi10Mg Aluminum Alloy $11.50 - $12.50 ¥78 - ¥85 Supplier quotation
EXW
Aluminum Alloy AlSi10Mg Aluminum Alloy $12.00 - $12.00 ¥82 - ¥82 Supplier quotation
EXW
Aluminum Alloy AlSi10Mg Aluminum Alloy $12.00 - $13.50 ¥82 - ¥92 Supplier quotation
EXW
Aluminum Alloy AlSi10Mg Aluminum Alloy $12.00 - $13.50 ¥82 - ¥92 Supplier quotation
EXW
Aluminum Alloy AlSi10Mg Aluminum Alloy $12.50 - $15.00 ¥85 - ¥102 Supplier quotation
EXW
Aluminum Alloy AlSi10Mg Aluminum Alloy $12.50 - $13.50 ¥85 - ¥92 Supplier quotation
EXW
Aluminum Alloy AlSi10Mg Aluminum Alloy $12.50 - $15.00 ¥85 - ¥102 Supplier quotation
EXW
Aluminum Alloy AlSi10Mg Aluminum Alloy $12.50 - $15.00 ¥85 - ¥102 Supplier quotation
EXW
Aluminum Alloy 6061 Aluminum Alloy $12.50 - $15.00 ¥85 - ¥102 Supplier quotation
EXW
Aluminum Alloy AlSi10Mg Aluminum Alloy $13.50 - $15.00 ¥92 - ¥102 Supplier quotation
EXW
Aluminum Alloy AlSi10Mg Aluminum Alloy $13.50 - $16.50 ¥92 - ¥112 Supplier quotation
EXW
Aluminum Alloy 6061 Aluminum Alloy $15.00 - $25.00 ¥102 - ¥170 Supplier quotation
EXW
Stainless Steel 7075 Aluminum Alloy $18.00 - $26.50 ¥122 - ¥180 Supplier quotation
EXW
Aluminum Alloy 2024 Aluminum Alloy $19.50 - $34.00 ¥133 - ¥231 Supplier quotation
EXW
Stainless Steel 4Cr13 Martensitic Stainless Steel $21.00 - $24.00 ¥143 - ¥163 Supplier quotation
EXW
Stainless Steel H13 Hot Work Tool Steel $21.00 - $24.00 ¥143 - ¥163 Supplier quotation
EXW
Stainless Steel 20Cr13 Stainless Steel $21.00 - $24.00 ¥143 - ¥163 Supplier quotation
EXW
Stainless Steel 17-4PH Stainless Steel $21.00 - $24.00 ¥143 - ¥163 Supplier quotation
EXW
Stainless Steel GCr15 Bearing Steel $21.00 - $24.00 ¥143 - ¥163 Supplier quotation
EXW
Stainless Steel 42CrMo Alloy Steel $21.00 - $24.00 ¥143 - ¥163 Supplier quotation
EXW
Aluminum Alloy 6061 Aluminum Alloy $22.50 - $34.00 ¥153 - ¥231 Supplier quotation
EXW
Stainless Steel DT4C Pure Iron $26.50 - $32.50 ¥180 - ¥221 Supplier quotation
EXW
Stainless Steel DT4C Pure Iron $26.50 - $32.50 ¥180 - ¥221 Supplier quotation
EXW
Stainless Steel DT4C Pure Iron $26.50 - $32.50 ¥180 - ¥221 Supplier quotation
EXW
Aluminum Alloy 7075 Aluminum Alloy $26.50 - $38.50 ¥180 - ¥262 Supplier quotation
EXW
Stainless Steel 316L $29.50 - $37.50 ¥201 - ¥255 Supplier quotation
EXW
Aluminum Alloy AlSi10Mg Aluminum Alloy $32.50 - $34.00 ¥221 - ¥231 Supplier quotation
EXW
Tool Steel 18Ni300 $37.00 - $48.00 ¥252 - ¥327 Supplier quotation
EXW
Aluminum Alloy AlSi10Mg $40.50 - $51.50 ¥276 - ¥350 Supplier quotation
EXW
Nickel Alloy GH4169 / Inconel 718 Nickel Superalloy $44.50 - $49.00 ¥303 - ¥333 Supplier quotation
EXW
Titanium Alloy TC11 Titanium Alloy $44.50 - $51.50 ¥303 - ¥350 Supplier quotation
EXW
Titanium Alloy TA15 Titanium Alloy $44.50 - $49.00 ¥303 - ¥333 Supplier quotation
EXW
Titanium Alloy TA15 Titanium Alloy $46.00 - $49.00 ¥313 - ¥333 Supplier quotation
EXW
Titanium Alloy TC11 Titanium Alloy $50.50 - $54.50 ¥344 - ¥371 Supplier quotation
EXW
Copper Alloy CuCrZr Copper Alloy $50.50 - $66.50 ¥344 - ¥452 Supplier quotation
EXW
Nickel Alloy GH3625 / Inconel 625 Nickel Superalloy $51.50 - $53.00 ¥350 - ¥361 Supplier quotation
EXW
Nickel Alloy GH3625 / Inconel 625 Nickel Superalloy $62.00 - $66.50 ¥422 - ¥452 Supplier quotation
EXW
Nickel Alloy GH3625 / Inconel 625 Nickel Superalloy $62.00 - $66.50 ¥422 - ¥452 Supplier quotation
EXW
Copper Alloy CuCrZr Copper Alloy $62.00 - $66.50 ¥422 - ¥452 Supplier quotation
EXW
Copper Alloy CuCrZr Copper Alloy $62.00 - $62.00 ¥422 - ¥422 Supplier quotation
EXW
Aluminum Alloy AlMgScZr High-Strength Aluminum Alloy $62.00 - $74.00 ¥422 - ¥503 Supplier quotation
EXW
Copper Alloy CuCrZr Copper Alloy $66.50 - $71.00 ¥452 - ¥483 Supplier quotation
EXW
Nickel Alloy GH4099 Nickel Superalloy $81.00 - $88.50 ¥551 - ¥602 Supplier quotation
EXW
Titanium Alloy Ti-6Al-4V (Grade 5) $90.00 - $101.50 ¥612 - ¥690 Supplier quotation
EXW
Nickel Alloy Inconel 718 (GH4169) $128.00 - $149.50 ¥871 - ¥1017 Supplier quotation
EXW
Titanium Alloy Ti-6Al-4V ELI (Grade 23) $159.00 - $191.50 ¥1082 - ¥1303 Supplier quotation
EXW
Aluminum Alloy AlMgSc (Scalmalloy) $171.00 - $213.50 ¥1163 - ¥1452 Supplier quotation
EXW
Nickel Alloy GH5188 Cobalt-Based Superalloy $176.50 - $176.50 ¥1201 - ¥1201 Supplier quotation
EXW
Cobalt-Chrome CoCrMoW $191.50 - $235.50 ¥1303 - ¥1602 Supplier quotation
EXW

Data Methodology: Prices are collected from supplier quotations on PowderSight platform and synced from the domestic Chinese database. CNY prices are supplier-declared EXW prices. USD prices are converted at the daily CNY/USD exchange rate from ExchangeRate-API. Last sync: daily at 02:00 CST.